| Category | Type | Grade | Thickness (mm) |
|---|---|---|---|
| Non-Oriented | Common series | 35SW230 35SW250 35SW270 35SW300 35SW330 35SW360 35SW400 35SW440 | 0.35 |
| 50SW230 50SW250 50SW270 50SW290 50SW310 50SW330 50SW350 50SW400 50SW470 50SW530 50SW600 50SW700 50SW800 50SW1000 50SW1300 | 0.5 | ||
| 65SW600 65SW700 65SW800 65SW1000 65SW1300 | 0.65 | ||
| High efficiency series | 50SWH470 50SWG470 50SWH600 50SWH800 | 0.5 | |
| Stress-relief annealing series | 35SWR300 | 0.3 | |
| 50SWR350 50SWR1300 | 0.5 | ||
| Medium frequency series | 20SW1500 | 0.2 | |
| 27SW2300 | 0.27 | ||
| 30SW2700 | 0.3 | ||
| Oriented | Common type | 23SQ110 | 0.23 |
| 27SQ110 27SQ120 | 0.27 | ||
| 30SQ120 30SQ130 | 0.3 | ||
| 35SQ135 35SQ145 35SQ155 | 0.35 | ||
| High induction type | 23SQG085 23SQG090 23SQG095 | 0.23 | |
| 27SQG090 27SQG095 27SQG100 | 0.27 | ||
| 30SQG100 30SQG105 30SQG110 30SQG120 | 0.3 | ||
| 35SQG115 35SQG125 35SQG135 | 0.35 | ||
| Domain refined high induction type | 23SQGD80 23SQGD85 23SQGD90 | 0.23 | |
| 27SQGD85 27SQGD90 27SQGD95 | 0.27 | ||
| 30SQGD95 30SQGD100 30SQGD105 | 0.3 |
Non-Oriented electrical steel has magnetic properties that are uniform in all directions, making it ideal for rotating machinery like motors and generators. Oriented electrical steel is processed to optimize magnetic performance in a single direction, making it suitable for static applications like transformers.
Our Non-Oriented electrical steel comes in various thicknesses depending on the series, including 0.2mm, 0.27mm, 0.3mm, 0.35mm, 0.5mm, and 0.65mm, catering to different operational frequency needs.
High Efficiency series grades reduce iron loss and increase power output efficiency. Stress-Relief Annealing series allow for stress release after mechanical stamping, optimizing magnetic permeability and reducing core losses during operation.
Domain Refined High Induction steel offers ultra-low core loss and superior magnetic flux density, specifically designed for ultra-high voltage (UHV) transformers, large power transformers, and high-efficiency power distribution systems.
Selection depends on your operating frequency, target efficiency, allowable iron loss, and working environment. Thinner laminations (e.g., 0.2mm - 0.35mm) are typically chosen for high-frequency or high-efficiency applications to minimize eddy current losses.